The principle behind NDT-RAM is simple. Every part has a unique resonant signature or pattern that reflects its composition. Any deviation from the expected signature indicates the presence of structural inconsistencies commonly due to flaws or mechanical variations. An intuitive example is a cracked bell that no longer sounds quite right, lacking a clear ring and unable to hold its tone.