_DSC8700_Lynx.jpgThe ISOVOLT Lynx is the first in a new generation of stationary X-ray machines from GE Measure-ment & Control. It represents a major advance in X-ray generator technology, incorporating the latest electronics and digital concepts to allow greater performance and reliability. It has been designed to align with the optimized performance of other components in the X-ray inspection imaging chain for a wide range of applications including the automotive, aerospace and metals manufacturing sectors, for tasks such as the inspection of welds, composites and castings, as well as in 3-D computed tomography and metrology. It will be of particular interest to system integrators working in both the industrial and scientific sectors.