Shimadzu’s HMV-G Series of Micro Vickers hardness testers provide an operator-friendly, cost-effective solution for a wide range of testing applications. They feature a CCD camera for automatic length measurement, an automatic lens switching function, sample shape recognition function, and a newly designed frame that dramatically improves operability.