One of the most fundamental decisions in mechanical design is selecting which material a part should be produced from. Often, a variety of factors will influence the success of a part: strength, elasticity, durability, machining requirements, cost… not to mention electrical, thermal, and chemical effects can also conspire against ongoing part performance and longevity.

This may sound daunting, but material selection has been greatly simplified through advancements in our understanding of material properties. Countless material properties that characterize almost every imaginable dimension are now organized within digital catalogs to provide engineers with quick insights as to how a given material should behave when put into service.

As an entrée into the world of material science, let us take a step back to focus on a couple of key terms: material properties and—the empirical basis of material properties—materials testing.


Material Properties

QM 0222 Quality 101 F305 Wedge Grips

An advanced force tester is a rigidly constructed vertical frame with integrated control panel, force sensor, and grips appropriate to the application. Source: Mark-10

The scope of this discussion will be limited to mechanical applications. But, speaking more broadly, material properties can also characterize electrical, thermal, and chemical behaviors, too.

Since material properties can characterize such a wide range of attributes, countless performance predictions can be made through mere calculation. Calculations can be as easy as arithmetic or they can require advanced software that will map material properties over irregular geometries and then churn through simulations. These calculations are convenient as they give engineers a ballpark idea of how a design might perform—and long before that prospective part tangibly exists.

But any estimate of this kind will be confronted by some inherent limitations. Regardless of how sophisticated the calculations might be, these predictions remain merely theoretical and cannot fully account for the natural complexity of the physical world. Responsibility should demand that we confirm theoretical predictions with actual empirical data.


QM 0222 Quality 101 Graph View

A typical graphical representation of a materials test. Three recent runs are compared for consistency. Source: Mark-10 (Click on the image to enlarge.)


Materials Testing

Physical materials testing allows engineers to decimate the residual uncertainties that haunt simulation results. So, despite the undeniably impressive power of modern computing, real-life materials testing remains necessary to validate the materials that comprise critical componentry.

But this is not to say computers have no place within material testing. To properly evaluate the mechanical attributes and behaviors of a material, an advanced force tester can be employed. Traditionally known as a materials testing machine, an advanced force tester relies on an integrated computer paired with a motion controller to orchestrate a series of test stages, automatically capture and calculate predefined test results, and generate graphical representations of the loading event.

By having an integrated computer continuously monitor each aspect of the test as it unfolds while controlling crosshead motion in real-time, operator influence is sidelined to maximize the repeatability and reproducibility of test results.


QM 0222 Quality 101 F305 G1103 Wire Pull Test

Adhesive properties can be measured by subjecting a tape sample to a 90° peel test. Source: Mark-10 (Click on the image to enlarge.)


Peel Resistance Tests

Take, for example, the ever-popular material tests that examine peel resistance. Intuition might suggest these tests would be quite simple: just peel something resembling a piece of tape at a fixed speed and capture the peak force that occurred while removing it from some surface. In this scenario, capturing the peak force that occurred during the peel would tell us how much force was required to break the seal at its very strongest point. But—come to think of it—do seals always fail because their very strongest point was not strong enough?

It turns out, evaluating the strength of a seal is actually not so simple. These tests typically aim to determine both the average force that occurred over a given length of peel and also the minimum force that occurred over that same length. Complicating matters further, test methods usually insist that the advanced force tester ignores the beginning and end of the peel to only consider some predefined segment in the middle:

QM 0222 Quality 101 p5 Graph

The results of a peel resistance test are expressed as a ratio. Most often, it is the ratio between the average force that occurred during the peel divided by the width of the sample:

QM 0222 Quality 101 Equation 1 Peel Resistance

The peel resistance ratio of an adhesive allows an engineer to easily approximate the average force a given seal would be able to sustain by just knowing the width of that seal. The convenience of this quick calculation begs the question: why test at all when an engineer could just knock out some arithmetic on the back of a napkin?

In some basic-use cases, this approach might work out just fine. However, what if the application requires the adhesive to be applied a different substrate? Or perhaps an accelerant or coloring agent is added to the formulation? Or maybe the assembly will be taken outside of the normal temperature, humidity, or pressure criteria? Or imagine a circumstance where the adhesive manufacturer publishes performance specifications that omit the tolerances and uncertainties that engineers need to develop a defensible risk profile.

These everyday concerns are excellent reasons why an engineer or quality control professional would enjoy the assurance of designing their own material tests.


Creep Rate And Relaxation Rate Tests

Another common testing genre that typically requires the sophistication of an advanced force tester is creep and relaxation rate testing. Creep and relaxation properties both essentially characterize the same phenomenon: increasing mechanical compliance over time, but approached from opposite dimensions.

Creep Rate

Creep rate tests apply a fixed load to a sample and then hold that load constant for some predefined duration of time; this action is designed to emulate the constant force created by a weight placed atop a sample or pulling downward on the sample. During the hold period, the advanced force tester must constantly measure and record the ongoing change in sample deflection that continually occurs. It will present the creep rate as sample deflection per unit of time, as the following formula describes:

QM 0222 Quality 101 Equation 2 Creep Rate

As far as most mechanical tests go, creep rate testing requires the advanced force tester to compute the derivative of sample deflection taken with respect to time. This produces a test result that is dimensioned as a slow speed. And, since most creep and relaxation rates are nonlinear, the method by which this rate of change is calculated can dramatically impact the value, meaning, and reproducibility of test results.

Relaxation Rate

Like creep rate, relaxation rate examines the time function of material compliance. But relaxation rate tests swap the roles of force and displacement by holding sample displacement constant while measuring the load decay.

Relaxation rate tests also typically start out by applying some predefined load, but the purpose of this load is merely to create a known and repeatable datum point. Once this datum has been established, the advanced force tester then switches from controlling force to controlling position. After this transition, the advanced force tester will either hold the sample in its current position over some duration of time or it will deflect the sample some additional distance and then hold that new position constant. Either way, in the final step of this test, the advanced force tester will continuously measure the decay in load over the hold time and calculate test results.

Comparing the creep and relaxation rate equations, one can see how force and distance switch roles:

QM 0222 Quality 101 Equation 3 Relaxation Rate

The results of creep and relaxation rate tests have sweeping consequences. For a moment, just let every load-bearing application you can think of scroll through your mind: this could be everything from the exotic materials used in automotive and aerospace applications, to essentially every construction material in use, down to an ordinary stack of plastic bottles or cardboard boxes that must withstand palletization… the implications are everywhere. While creep and relaxation rates may not garner the excitement of, say, the ultimate tensile strength specification, their subtle importance is nearly ubiquitous.


In Summary

This discussion of material properties and material testing intends to drive home that, while cataloged material properties do indeed expedite the design process, they leave engineers and quality folks with an incomplete understanding of ultimate part performance.

To reach a high level of confidence before unveiling a product, the material content of that product should be subjected to tests that emulate its prospective service life and generate applicable test results. An advanced force tester’s configurability, repeatability, and reproducibility make it an indispensable tool in validating the mechanical attributes of parts, assemblies, and their constituent materials.